SYMASORB SMS
effects and function as filter medium.
APPLICATIONS
The crude polyols, after being blended with about 5%wt of water at 80~90°C for 15 minutes, are reacted with H3PO4 (a little more than the crude polyols in amount) for 1 hour, with the pH value of the neutralization solution controlled between 5.0~5.5.
At this stage, 1%wt of SYMASORB SMS is added into and blended with the solution while heating the temperature to 105°C~115°C .
Then dehydrate the solution at the speed from slow to quick in order to make the KH2PO4 crystals well-roportionally formed.
The dehydration process ends when the moisture reaches to minimum amount e.g. 0.05%wt. The filtering circulation follows and continues for 1 hour at the temperature of 105°C~115°C, pressure at 2~4Kpa. Analyze the content of K+(Na+). Filtration begins
Allgemeine Eigenschaften
Richten Sie ein kostenloses Prospector-Konto ein, um Zugang zu sämtlichen Angaben des Produktdatenblatts von SYMASORB SMS zu erhalten. Dort finden Sie alle Angaben zu den physikalischen, mechanischen und Härteeigenschaften
Technical Datasheet (English)
Dokument herunterladenVerarbeitung
Finden Sie bestimmte Informationen zur Verarbeitung für SYMASORB sowie allgemeine Informationen zum allgemeinen Produktkreis Additive -- Slip Agent / Lubricant / Mold Release / Processing Aid. Registrieren oder Anmelden um mehr Informationen erhalten.
Bezugsquellen
Sie können SYMASORB SMS von 1 Händler(n) oder Hersteller(n) kaufen. Registrieren oder Anmelden um mehr Informationen erhalten.
PROSPECTOR
Finden Sie Lösungen, nicht nur Materialien.
Wenn Sie sich bei Prospector registrieren, können Sie unsere dynamischen Werkzeuge und Funktionen nutzen, um schnell Lösungen zu finden.
Noch heute registrieren