SYMASORB SMS
effects and function as filter medium.
APPLICATIONS
The crude polyols, after being blended with about 5%wt of water at 80~90°C for 15 minutes, are reacted with H3PO4 (a little more than the crude polyols in amount) for 1 hour, with the pH value of the neutralization solution controlled between 5.0~5.5.
At this stage, 1%wt of SYMASORB SMS is added into and blended with the solution while heating the temperature to 105°C~115°C .
Then dehydrate the solution at the speed from slow to quick in order to make the KH2PO4 crystals well-roportionally formed.
The dehydration process ends when the moisture reaches to minimum amount e.g. 0.05%wt. The filtering circulation follows and continues for 1 hour at the temperature of 105°C~115°C, pressure at 2~4Kpa. Analyze the content of K+(Na+). Filtration begins
Propiedades generales
Acceda a los detalles completos de la hoja de datos de SYMASORB SMS cuando cree su cuenta gratuita con Prospector. Encontrará información completa sobre especificaciones físicas, mecánicas y de dureza
Technical Datasheet (English)
Descargar documentoProcesando
Encuentre información de procesamiento específica para SYMASORB, así como información general para la familia genérica de Additive -- Slip Agent / Lubricant / Mold Release / Processing Aid. Registrarse o Iniciar sesión para obtener más información.
Dónde comprar
Puede comprar SYMASORB SMS de 1 distribuidores o fabricantes. Registrarse o Iniciar sesión para obtener más información.
PROSPECTOR
Encuentre soluciones, no solo materiales.
Cuando se une a Prospector, aprovecha las herramientas y funciones dinámicas para encontrar soluciones rápidamente.
Regístrese hoy