SYMASORB SMS
effects and function as filter medium.
APPLICATIONS
The crude polyols, after being blended with about 5%wt of water at 80~90°C for 15 minutes, are reacted with H3PO4 (a little more than the crude polyols in amount) for 1 hour, with the pH value of the neutralization solution controlled between 5.0~5.5.
At this stage, 1%wt of SYMASORB SMS is added into and blended with the solution while heating the temperature to 105°C~115°C .
Then dehydrate the solution at the speed from slow to quick in order to make the KH2PO4 crystals well-roportionally formed.
The dehydration process ends when the moisture reaches to minimum amount e.g. 0.05%wt. The filtering circulation follows and continues for 1 hour at the temperature of 105°C~115°C, pressure at 2~4Kpa. Analyze the content of K+(Na+). Filtration begins
Propriétés générales
Consultez la fiche technique complète de SYMASORB SMS en créant gratuitement votre compte Prospector. Vous y trouverez des informations exhaustives sur les propriétés physiques et mécaniques et sur la dureté
Technical Datasheet (English)
Télécharger le documentTraitement en cours
Find specific processing information for SYMASORB as well as general information for the Additive -- Slip Agent / Lubricant / Mold Release / Processing Aid generic family. S’inscrire ou Connexion pour en savoir plus.
Où acheter
Vous pouvez acheter SYMASORB SMS auprès de 1 distributeurs ou fabricants. S’inscrire ou Connexion pour en savoir plus.