SYMASORB SMS
effects and function as filter medium.
APPLICATIONS
The crude polyols, after being blended with about 5%wt of water at 80~90°C for 15 minutes, are reacted with H3PO4 (a little more than the crude polyols in amount) for 1 hour, with the pH value of the neutralization solution controlled between 5.0~5.5.
At this stage, 1%wt of SYMASORB SMS is added into and blended with the solution while heating the temperature to 105°C~115°C .
Then dehydrate the solution at the speed from slow to quick in order to make the KH2PO4 crystals well-roportionally formed.
The dehydration process ends when the moisture reaches to minimum amount e.g. 0.05%wt. The filtering circulation follows and continues for 1 hour at the temperature of 105°C~115°C, pressure at 2~4Kpa. Analyze the content of K+(Na+). Filtration begins
Propriedades gerais
Acesse os detalhes completos da ficha de dados de SYMASORB SMS quando você criar sua conta gratuita no Prospector. Você encontrará informações completas sobre especificações físicas, mecânicas e de dureza
Technical Datasheet (English)
Baixar o documentoProcessamento
Encontre informações de processamento específicas para SYMASORB, além de informações gerais para a família genérica Additive -- Slip Agent / Lubricant / Mold Release / Processing Aid. Inscreva-se ou Faça login para mais informações.
Onde comprar
Você pode adquirir SYMASORB SMS de 1 distribuidores ou fabricantes. Inscreva-se ou Faça login para mais informações.
PROSPECTOR
Encontre soluções, não somente materiais.
Quando se junta ao Prospector, você se beneficia de recursos e ferramentas dinâmicas para encontrar soluções rapidamente..
Inscreva-se hoje mesmo